there is several reasons this happens. First some water based sealers use a fluro that is slightly acidic. Second some will also leave a residue on the surface. If its a true etch, Ph is the only reason it will etch, unless its an alkaline etch
This happened to me using VMC Kleerseal a long time ago, when flouro polymer technology was new and this was one of the first of these type sealer, water based. Don’t know why it happened but it was very noticable.
From: rosen.stuart@gmail.com [mailto:rosen.stuart@gmail.com] On Behalf Of stuart rosen
Sent: Friday, July 17, 2009 1:00 PM
To: Restoration and Maintenance
Subject: [sccpartners] water based sealer etched stone
last year I used a water based sealer witch our customer spec out for us.We sprayed the sealer on limestone and it caused very light etching.We had only just began when we caught it so it was easy to correct.When I read the back of the bottle the instructions
mentioned some stones can be etched by using this product.Showed that to the customer and got the ok to use a product that we knew.
Anyway just heard a story that it happened to someone else only with a different water based sealer. I think siloxanes are corrosive (high alkaline) when not diluted.
But I know that diluted in a sealer they are in small amounts so its not normal for this to occur. Does anyone know why it does occur. Has anyone else had this happen to them?
--
Regards,
Stu Rosen
201-446-1200
www.mbstone.com
www.stoneshine.com
"A posse ad esse "
Powered by http://DiscussThis.com
Visit list archives, subscribe, unsubscribe or change your subscription preferences
Start a new conversation (thread)