You can also mix the slurry with an acrylic mortar additive.

Sent via BlackBerry® from Telstra


From: Phil Campbell <phil@campbellsstonerestoration.com>
Sender: phlchr@gmail.com
Date: Wed, 7 Jul 2010 11:40:18 -0500
To: Restoration and Maintenance<sccpartners@stoneandtilepros.com>
ReplyTo: "Restoration and Maintenance" <sccpartners@stoneandtilepros.com>
Subject: [sccpartners] Question

I'm honing a Jerusalem stone floor and it has some pitting on about 6 stones, some of the pits are the size of a quarter and about 1/8 inch deep, it's at the entrance so could be spalling from salts. I can't find replacement stones quick enough they are 6"x15"x2cm. to match the color could I use the dried surry from the honing process? There's enough pitting that I think epoxy would show, I do ok with polyester but this floor has that dull shiny look so I not sure about the epoxy finish look. Thanks Phil
 
Campbell's Stone Restoration
Stone CSI
Certified Stone Inspector

Powered by http://DiscussThis.com
Visit list archives, subscribe, unsubscribe or change your subscription preferences
Start a new conversation (thread)