Randy,

 

Going up to 3000 is over kill, the serpentine has some calcium in it so there will be a polishing reaction using the 5X polishing Powders. The crystallizer will just give it the final pop to the finish.

Also not all crystallizers are pink.

 

 

John E. Freitag

President/Director

The Stone and Tile School

Office 407-567-7652

Cell 407-615-0134

jfreitag@thestoneandtileschool.com

 

schoollogo

 

www.thestoneandtileschool.com

 

 

 

From: Randy Frye [mailto:rfrye@comcast.net]
Sent: Wednesday, July 06, 2011 8:00 AM
To: Restoration and Maintenance
Subject: RE: [sccpartners] No subject

 

We start at the appointed grit, carry the grits to at least 3000, then granite polishing paste, finalize with the pink stuff.
Good luck


On 7/6/11 1:20 AM, "Roger Konarski" <qm144@yahoo.com> wrote:

I have been asked to restore a serpentine bathroom. Shower, vanity top, tub surround and floor. This is one stone I don't like to restore. Looking for suggestions on handling this job. Honing followed with MB 20 or should we just use the pink stuff on the stone?
 
Thanks,
RK  


Powered by http://DiscussThis.com <http://www.discussthis.com>
Visit list archives, subscribe, unsubscribe or change your subscription preferences  <http://www.discussthis.com/members/sccpartners@stoneandtilepros.com>
Start a new conversation (thread) <mailto:sccpartners@stoneandtilepros.com>


Powered by http://DiscussThis.com
Visit list archives, subscribe, unsubscribe or change your subscription preferences
Start a new conversation (thread)