Re: [sccpartners] Densifier
Kris Dougherty 06 May 2011 11:04 EDT
I would just test my densifier down in a small area and let it stay wet
for 20 to 30 min. Then dry for 1 hour or more then polish the floor as a
test section. To reapply more densifier should not be a problem if the
floor has been densified prior. This should work fine.
Kris
Marble Floors and More
On 5/6/2011 9:17 AM, flooramor@aim.com wrote:
> Fellow colleagues,
>
> How do you test for densifier? Looking at a terrazzo floor from the 1960s that has already been polished before, but is obviously now showing signs of wear and abuse, mainly in the traffic areas. It has a nice sheen in some areas but not a lot of clarity.
>