Transition from 220 metal
Scott Wilson 29 Aug 2015 11:04 EDT
Hi partners
In florida most of my work is travertine or terrazzo
I have done around 50000 sq ft of polished concrete in the last 5 years,with good success
45,70.120 metal, to 50 resin ,just to make sure I got all the scratches
This time I used metals to 220
Do I need to transition back to 100 resins, or will good quality 200 resin make the transition
Without residual scratches?
Blessings All
Scott Wilson